Comment by buildsjets 13 hours ago How comfortable are you working with chromic acid and boric-sulfuric acid in your home? 3 comments buildsjets Reply mmsc 11 hours ago As long as it's not hydrofluoric acid... wereHamster 10 hours ago I bought a light HF acid (rust remover) so I can properly clean titanium parts before anodizing. Worked like a charm... cultofmetatron 7 hours ago just don't let any of it get on your skin. only takes a splash to land you in intensive care.
mmsc 11 hours ago As long as it's not hydrofluoric acid... wereHamster 10 hours ago I bought a light HF acid (rust remover) so I can properly clean titanium parts before anodizing. Worked like a charm... cultofmetatron 7 hours ago just don't let any of it get on your skin. only takes a splash to land you in intensive care.
wereHamster 10 hours ago I bought a light HF acid (rust remover) so I can properly clean titanium parts before anodizing. Worked like a charm... cultofmetatron 7 hours ago just don't let any of it get on your skin. only takes a splash to land you in intensive care.
cultofmetatron 7 hours ago just don't let any of it get on your skin. only takes a splash to land you in intensive care.
As long as it's not hydrofluoric acid...
I bought a light HF acid (rust remover) so I can properly clean titanium parts before anodizing. Worked like a charm...
just don't let any of it get on your skin. only takes a splash to land you in intensive care.